Wrinkles on the vamps – Case #040

November 9, 2012

by

“A picture is worth a thousand words”. Practical solutions to problems encountered in the manufacturing process that demonstrate how we assist our customers’ factories to produce  Right from the Start TM.

Problem: wrinkles on the Vamp during crimping operation.

Impactiva solution: we got the factory to use a 1.5 mm EVA foam on the lining side during the vamp crimping operation in order to avoid impressions.

Stay tuned for more Impactiva technical solutions to every day production problems.